Why Glassy Phase Exudation Matters in AZS Blocks

Sep 30, 2026

Leave a message

When glass quality is critical, choosing AZS blocks by zirconia content and price alone leaves an important question unanswered: how will the material behave when heated? Glassy phase exudation is one property worth discussing before an order, because material released from the refractory can become a source of glass defects.

info-1446-750

High-temperature laboratory work shown in Dezhong company materials. Test conditions must accompany reported results.

 

For fused cast alumina-zirconia-silica (AZS) blocks, an exudation figure is meaningful only with its test conditions and sample information. This guide explains the property, shows examples from Dezhong testing materials and sets out what an overseas buyer should ask before comparing reports.

 

Dezhong has glassy phase exudation testing capability. The applicable test procedure, sampling plan and acceptance requirements should be confirmed for the product and order.

 

What glassy phase exudation means

 

The term describes glassy material already present in the AZS refractory moving out toward its surface during heating. It does not mean that the entire block melts, and it is different from external molten glass penetrating a brick. Exuded material may reach the glass bath from glass-contact blocks or from structures above it.

info-1446-1477

Specimen marked 41# in Dezhong exudation-test materials. The original 2023 date is retained; this photograph is not a numerical test report.

 

Exudation can contribute to defects such as cords or stones, making it relevant to glass quality, including during early furnace service. This is a reason to assess the risk, not evidence that every observed glass defect comes from AZS. Defect diagnosis needs information about the glass and furnace operation as well as the refractory.

 

The specimen image illustrates what Dezhong has documented. Without the measurement record and acceptance basis, its surface appearance alone cannot establish an exudation percentage or a pass result.

 

Compare the test conditions before the numbers

 

Two reports carrying the same property name may not measure it in the same way. Use the following items to check whether the results can be compared. A lower number is useful only when the method and relevant conditions are comparable.

Report item

What the buyer should confirm

Method and version

The named standard or agreed procedure, including any deviations.

Thermal programme

Temperature, hold time, heating and cooling conditions, and number of cycles.

Sample identity

Grade, batch, sampling position, specimen dimensions and preparation.

Result definition

What the reported number measures, its unit and calculation basis.

Acceptance basis

Whether the value is a typical value, a measured result or an agreed limit.

 

For example, the public scope of ASTM C1223 describes a result based on specimen volume increase after cooling. That percentage should not be read as the total glassy phase content of the original block. Naming ASTM C1223 here does not mean that every Dezhong test follows it; the actual procedure must be confirmed.

 

Keep typical catalogue values separate from actual sample results and contractual limits. A single result should retain its grade, batch and sampling reference rather than becoming a claim about every block supplied.

 

Exudation and corrosion are different checks

 

An exudation test evaluates the release of the refractory glassy phase under its specified heating procedure. A glass-corrosion test evaluates material attack by the test glass under defined conditions. A blistering test investigates bubble-generation tendency. These results answer different questions and should not replace one another.

info-1446-983

Static glass-corrosion specimen shown in Dezhong materials. It illustrates a separate test, not an exudation measurement.

 

Dezhong company materials show an exudation-test example labelled 1500°C for 4 hours. The same presentation separately identifies a static glass-corrosion example at 1500°C for 36 hours. The longer duration belongs to the corrosion example, not to the exudation photograph.

 

These example conditions are not a complete protocol, an acceptance limit or a maximum service-temperature rating. Dezhong capabilities include exudation and corrosion testing. Confirm the full method and reporting scope for your order, and discuss whether additional glass-contact tests are needed and how they would be arranged.

 

Turn test information into a clear enquiry

 

Q: Does low exudation guarantee defect free glass

A: No single refractory test can guarantee the quality of all finished glass. Exudation is one part of material assessment. Glass composition, the application position and operating conditions still matter. When investigating a production problem, provide the defect type and operating history rather than assigning the cause from one photograph.

Q: Can a sample result be applied to the whole shipment

A: Its relevance depends on the sampling and acceptance plan. Ask which grade, batch and region the specimen represents, how many specimens were tested and how the result is connected to the order. Do not treat an undated sample photo as a current shipment report.

Q: What to send to Dezhong

A: Send the glass type or composition, furnace section, operating conditions, AZS grade if specified, drawings and quantities. Include your glass-quality concerns and any required test method or acceptance limit. If you are comparing supplier reports, retain their test conditions and units so the discussion is based on comparable evidence.

 

modular-1
Discuss your AZS testing requirements

Contact zzdz@dzrefactory.com to discuss the applicable product and inspection requirements. Agree on the procedure and reporting scope before acceptance, so that the test information helps answer your actual furnace and glass-quality questions.

 

 

 